1. Fine porosity would be remained in Powder metallurgy of processing for Tungsten Carbide, which will be the beginning of destroy of products.
2. To remove this fine porosity, we PASSION produce products through HIP Process.
3. This process is progressed under the high temperature and pressure, and put the identical pressure on whole surface of product.
4. At this time, a fine porosity would be removed, and effected on improving high strength.
No. |
Common Size(mm) |
Refer Picture |
1 |
193*18.9*0.884 |
|
2 |
170*19*0.884 |
|
3 |
140*19*1.4 |
|
4 |
140*19*0.884 |
|
5 |
135.5*19.05*1.4 |
|
6 |
135*19.05*1.4 |
|
7 |
135*18.5*1.4 |
|
8 |
118*19*1.5 |
|
9 |
117.5*15.5*0.9 |
|
10 |
115.3*18.54*0.84 |
|
11 |
95*19*0.884 |
|
12 |
90*10*0.9 |
|
13 |
74.5*15.5*0.884 |
|
Note:Customization available per customer's drawing or sample |
The blade is suitable for ordinary film, plastic film, winding film cutting, PE cutting and other materials slitting.